Explain the wiring method of high-voltage test transformer

Explain the wiring method of the high voltage test transformer:

1, according to the wiring diagram to connect the working line, it must be noted that the use of the test transformer must be "high voltage tail" and reliable grounding.

2. Before turning on the power, adjust the regulator of the operation box (Taiwan) to zero. After the power is turned on, the green indicator light is on, the start button is pressed, and the red indicator light is on, indicating that the transformer is powered on and waiting for boost.

3. Rotate the pressure regulator handle clockwise with a speed of 1.5-2KV/S, and pay close attention to the meter indication and the condition of the tested product. When the leakage current is too large or the test product is broken down, overcurrent protection The relay will quickly cut off the power supply.

4. After the oil-immersed test transformer is completed, adjust the pressure regulator to zero at a uniform speed.

5. If the voltmeter pointer is found to be oscillating during the test, the current meter indication value increases sharply, or the sample smokes, arcs, has a focal position, and abnormal noise, the voltage should be immediately depressurized, cut off the power source, and check the cause.

6. When the oil immersed test transformer is used for DC test, the high voltage test transformer shall loosen and loosen the silicon stack short circuit rod (D) and the series tapping terminal rod (C) in the high voltage sleeve, and wrap it with clean insulation paper. When conducting the AC voltage test after the DC test, two shorting rods must be screwed.

7. Current limiting resistors and filter capacitors should be added to the DC test to prevent damaging the silicon stack.

8, the environment; temperature is too high, the top of the casing may have a small amount of oil overflow, is a normal phenomenon. When the DC test, if the corona on the inner wall of the casing appears obvious, it is generally a phenomenon of low oil. At this time, the shorting rod should be taken out, and the qualified 25# transformer oil should be supplemented with a syringe from its hole.

9. When the test transformer is used in series, the high voltage test transformer must pay attention to the corresponding contact between the output terminals (A) and (X) of the operation box and the output terminals (a) and (x) of the first test transformer. The first test transformer The output terminals (A, X) are connected to the test transformer input terminals (a) and (x) on the second JT1. The housing of the test transformer should be connected to the input of the primary transformer, and the input terminal of the test transformer on the third JT2. (a) and (x) are connected to the top output terminals (A) and (X) of the test transformer bushing on the second JT1.

For more information, please contact us

Laser Cladding Powder

Nickel Based Laser Cladding Powder

Ni base alloy powder is mainly made of NiCrBSi or NiBSi. Ni-based self-fluxing powder has good wettability, corrosion resistance and high temperature self-lubricating effect, and is used in components with heat resistance, corrosion resistance and thermal fatigue resistance. In general Ni35,Ni45,Ni60 etc can be used for laser cladding, the No means hardness of powder. Inconel 625 and 718 has good corrosion property under higher temperature, also widely used for laser cladding process.


Cobalt based Laser Cladding Powder

Cobalt-based alloy powder is the cemented carbide resistant to various types of wear and corrosion as well as high temperature oxidation. That is, the so-called cobalt-chromium-tungsten (molybdenum) alloy or Stellite alloy cobalt-based alloy is mainly composed of cobalt, containing a considerable amount of nickel, chromium, tungsten and a small amount of molybdenum, niobium, tantalum, titanium, Alloying elements such as lanthanum, and occasionally a class of alloys containing iron.

Co-based self-fluxing alloys have good high temperature performance and wear resistance and corrosion resistance, and are used in petrochemical power, metallurgy and other industrial fields where they are wear-resistant, corrosion-resistant and high-temperature resistant.

Laser Cladding


Iron based Laser Cladding Powder

The work pieces required for laser cladding and manufacturing in the actual industry are mainly carbon steel and cast steel. The Fe-based alloy is close to the base material in composition and has good wettability. The advantage of Fe base powder is lower cost and good wear resistant of cladding layer. As a result, it`s the most widely used for laser cladding process. It is suitable for parts that require local wear resistance and are easily deformed.

Laser Cladding Work Part



WC blended Laser Cladding Powder

Tungsten carbide blended with Ni alloy powder is the best choice for wear resistant work piece. This unique process can bring excellent wear, corrosion and high temperature resistant. Our blend powder can achieve different portion of WC from 35% to 60% without crack under suitable cladding parameter.


Laser Cladding 2


Iron Alloy Powder,Nickel Alloy Powder,Cobalt Alloy Powder,Laser Cladding Powder